摘要
对影响活炉底复吹转炉使用寿命原因进行分析,通过对炉衬材质及砖型设计优化、复吹转炉砌筑工艺的优化、炉底底吹金属蘑菇头形成及维护、活炉底复吹转炉溅渣护炉及炉衬挂渣喷补维护等工艺措施,提高了120 t活炉底复吹转炉的使用寿命,炉龄达到27 000炉。
The reasons of affecting low service life were analyzed about the Combined blown converter with Movable furnace bottom,and through the design application of the lining-refractory and the brick shape, the laying process, the bottom of the furnace bottom blowing metal mushroom head formation and maintenance, slag splashing and the gunning maintenance, and so on, all these measures make the service life achieve 27 000 on 120 t Combined blown converter with Movable furnace bottom.
出处
《山东冶金》
CAS
2015年第5期26-28,共3页
Shandong Metallurgy
关键词
活炉底
复吹转炉
炉衬寿命
溅渣护炉
movable furnace bottom
combined blown converter
furnace lining life
slag splashing