易折型曲颈安瓿不易折断的原因分析 被引量:15

Analysis on Factors ThatCauses theDifficulties in Breaking-off the Easy-to-break Retort Ampoules
下载PDF
导出
摘要 针对易折型曲颈安瓿普遍存在不易折断的状况 ,对 13种易折型安瓿的非易折状况作了调查 ,并对 5所医院 335名临床护士就其操作现状进行了问卷调查。结果表明 :安瓿的非易折率最高达 78.4 8% ,护士在掰启易折型安瓿时仍需使用砂轮割锯。影响安瓿易折率最重要的因素是颈段的外直径与割痕长度 ,同规格间比较差异有显著性 (P<0 .0 1)。建议厂家要高度重视安瓿的质量 ,加强技术改革 ,提高易折型安瓿的易折率。 To counter that it is commonly hard to break off the easy-to-break ampoules, a survey of hard-to-break status of 13 kinds of easy-to-break ampoules was performed. Altogether 335 nurses from 5 hospitals were investigated by filling out the questionnaire about their manipulation process. Results showed that hard-to-break rate in some ampoules were as high as 78.48%. Nurses needed to use abrasive wheel cutter when they opened the easy-to-break ampoules. The most important factors that affecting the rate of easy-to-break of ampoules were both the outer diameter of the neck of ampoules and the length of cutting mark. There was a significant difference compared with each other in the same specification (P<0.01). Suggested that those companies should pay more attention to the quality of ampoules. They should strengthen their technological reform and elevate the quality of easy-to-break ampoules.
出处 《护理研究》 2002年第4期197-198,共2页 Chinese Nursing Research
关键词 易折型曲颈安瓿 颈外径 割痕长度 影响因素 易折率 Ampoule,easy-to-break type Quality Outer diameter of the neck Length of cutting mark
  • 相关文献

参考文献4

二级参考文献4

共引文献144

同被引文献113

引证文献15

二级引证文献48

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部