摘要 采用H2O2—微电解/Mn O2工艺处理造纸废水,研究了p H、铁炭用量、铁炭比、反应时间、Mn O2加入量、H2O2投加量等因素对处理效果的影响。结果表明,p H=3.0,铁炭总投加质量浓度为20 g/L,Mn O2投加质量浓度为2.50 g/L,H2O2投加质量浓度为0.55 g/L,铁炭物质的量比为1∶1,反应时间为50 min时,造纸废水的COD、SS、氨氮、总磷、BOD5的去除率分别为88%、98.4%、85%、98%、52%。同时可生化性由0.32提高到0.81,减小了后续生化处理工艺负荷。 H2O2-micro-electrolysis/MnO2 process has been used tor treating paper-making wastewater, i ne lmluences of the factors, such as pH,total iron and carbon, proportion of iron and carbon,reaction time, MnO2 dosage, H202 dosage,etc, on the removing effects are studied. The results show that when its pH is 3.0,total iron and carbon 20 g/L, MnO2 dosage 2.50 g/L,H202 dosage 0.55 g/L,ratio of iron and carbon 1:1 ,and reaction time 50 rain ,the removing rates of COD, SS, ammonia nitrogen, total phosphorous, BODs, can reach 88%, 98.4%, 85%, 98%, and 52%, respec- tively. The biodegradability is increased from 0.32 to 0.81. As a result, the load of subsequent biochemical treatment process is lightened.
作者 李长海
出处 《工业水处理》 CAS CSCD 北大核心 2015年第11期48-51,共4页 Industrial Water Treatment
基金 山东科技发展计划(2011GSF11713)
关键词 再生造纸废水 微电解 预处理 regenerated paper-making water micro-electrolysis pretreatment
  • 相关文献

参考文献13

二级参考文献105

共引文献141

同被引文献42

引证文献3

二级引证文献26

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部