摘要
用玻璃纤维桩树脂核(观察组)和铸造钻铬合金桩核(对照组)分别修复末端第二磨牙残冠各37颗。1-5年成功率,观察组分别为100%、100%、91.9%、86.5%、81.1%;对照组分别为97.3%、91.9%、83.8%、81.1%、73.0%,在5个时间点,2组桩核冠修复成功率差异均无统计学意义。
37 free second molar residual crowns were repaired by glass fiber post and resin core(GF group),and another 37 by cobalt chromium alloy casting post and core(CCA group).The success rate of 1 -5 years of GF group was 100%,100%,91.9%,86.5%and81.1%;that of CCA group 97.3%,91.9%,83.8%,81.1%and 73.0%,respectively(P〉0.05).
出处
《实用口腔医学杂志》
CAS
CSCD
北大核心
2015年第6期861-862,共2页
Journal of Practical Stomatology
基金
商丘市科技计划项目(编号:131161)
关键词
末端第二磨牙
残冠
玻璃纤维桩核
铸造钴铬合金桩核
Free second molar
Residual crown
Glass fiber post and core
Cobalt chromium alloy casting post and core