为确定某磁化水充填体的最佳磁化参数,利用两种方法来确定其最佳磁化条件,一是采用水泥活性系数,二是通过测定不同条件下充填体最大单轴抗压强度来确定,两者得到的结果是一致的。使用水泥活性系数得到最佳参数的时间比方法二早了28 d,说明利用水泥活性系数能够快速地得到磁化水的参数,提高了工作效率,可以广泛应用于实际生产中。
To determine its determine optimum magnetized parameters of magnetized water filling body, using two methods to optimum magnetization conditions, one is to use cement activity coefficient, the second is by measuring different filling body under the condition of maximum uniaxial compressive strength to determine. The results are consistent. Using cement activity coefficient to get the best parameters for 28 days earlier than method 2, which shows that using cement activation coefficient can quickly get the parameters of the magnetized water, improve the working efficiency. It can be widely used in practical production.