摘要
根据余热锅炉水冷壁腐蚀产生的原因,采取减少硫酸蒸汽、漏风等措施,避免锅炉水冷壁腐蚀爆管泄漏事故的发生。
According to the waste heat boiler waterwall corrosion reason, it takes measures of reducing sulfuric acid vapor, air leakage rate to avoid the burst of corrosion of boiler water wall tube leakage accident.
出处
《湖南有色金属》
CAS
2015年第6期48-50,共3页
Hunan Nonferrous Metals
关键词
水冷壁
爆管
酸蒸汽
漏风
腐蚀
water wall
tube explosion
acid steam
leakage
corrosion