用P204从废钒催化剂中萃取钒 被引量:5

Solvent Extraction of Vanadium from Waste Vanadium Catalyst with P204
下载PDF
导出
摘要 用P204+TBP+磺化煤油体系从废钒催化剂还原酸浸液中萃取回收钒,考察萃取相比(O/A)、P204浓度及待萃液初始pH对萃取钒的影响。结果表明,P204萃取钒最优条件为:萃取剂组成20%P204+10%TBP+70%磺化煤油、相比O/A=2、料液初始pH=2.2、萃取5 min。在此优化条件下,VO2+萃取率可达98.73%。用1.5mol/L硫酸反萃6min,VO2+反萃率达93.35%,且制得V2O5产品达GB 3283-1987冶金99级V2O5的标准。 Vanadium was extracted from acid reduction leaching solution of waste vanadium catalyst in P204+TBP+sulfonated kerosene system.The effects of phase ratio(O/A),P204 concentration and initial pH value of extraction solution on vanadium extraction were investigated.The results show that vanadium extraction rate is 98.73% under the optimum conditions including extraction system of 20%P204+10%TBP+70% sulfonated kerosene,O/A=2,initial pH value of feeding solution of 2.2,and extracting duration of 5min.Vanadium stripping rate is 89.91% with 1.5mol/L sulfuric acid as stripping agent for6 min.The final product of V2O5 could meet standard of GB 3283-1987 Metallurgical Grade 99V2O5.
出处 《有色金属(冶炼部分)》 CAS 北大核心 2016年第1期46-48,共3页 Nonferrous Metals(Extractive Metallurgy)
基金 湖北省高等学校青年教师深入企业行动计划项目(XD2012604)
关键词 P204 废钒催化剂 萃取 P204 waste vanadium catalyst solvent extraction vanadium
  • 相关文献

参考文献10

二级参考文献65

共引文献53

同被引文献62

引证文献5

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部