期刊文献+

感应加热淬火硬化层深度检测方法探讨 被引量:3

Discussion on detecting method for hardening depth of induction heating quenching
下载PDF
导出
摘要 针对淬硬层深的感应淬火工件,经过维氏硬度HV1与洛氏硬度HRA硬度分布及硬化层深度的对比检验证明,洛氏硬度计检验结果更具有真实性和代表性。 Counter to induction quenching workpiece with deeper hardened layer, both Vickers hardness(HV1) and Rockwell hardness(HRA) methods were used to comparatively detect its hardness distribution and hardening depth, it proved out that the detection results with Rockwell hardness tester were more real and representative.
出处 《哈尔滨轴承》 2015年第4期33-36,共4页 Journal of Harbin Bearing
关键词 感应淬火 硬化层深度 极限硬度 显微硬度HV1 洛氏硬度HRA induction quenching hardening depth limiting hardness Vickers hardness(HV1) Rockwell hardness(HRA)