摘要
采用表面探伤和超声波探伤方法对P92钢主蒸汽管道焊缝进行缺陷检测,能够有效的检验出气孔、夹渣、未熔合等类型缺陷,经挖补缺陷消除,通过科学的焊接工艺制定及严格的焊后热处理工艺控制,保证了焊接修复质量,消除了主蒸汽管道焊缝缺陷存在的隐患,为机组的安全运行提供了保证。
Surface detection and ultrasonic detection can be used to inspect the flaw on the welding seam of main steam pipe of P92 steel. The Haw types of air hole, slag inclusion, incomplete fusion, and so on, can be detected effectively, and then removed consequently by defect repair. The quality of welding repair can be guaranteed by constitution of scientific welding procedure and control of heat treatment process after welding. As a result, flaw hidden danger on the welding seam of main steam pipe can be removed to guarantee the safe operation of the units.
出处
《铸造技术》
CAS
北大核心
2016年第1期137-139,共3页
Foundry Technology
关键词
P92钢主蒸汽管道
缺陷检测
超声波探伤
焊接修复
main steam pipe of P92 steel
flaw inspection
ultrasonic detection
welding repair