摘要
针对PVC树脂在旋风干燥过程中容易出现杂质粒子数、挥发物质量分数超标的问题,进行了原因分析,并提出了解决措施:1干燥过程中实时监控产品性能,2及时隔离不合格树脂,3定期清理干燥系统,4定期更换空气过滤棉。
In order to solve the problem that impurity particle number and volatile matter mass fraction of PVC resin were sub-standard in cyclone drying process, reasons were analyzed, and improvement measures were proposed: (1)real time monitoring the above-mentioned performance during drying process, (2)in time separating unqualified PVC resin from qualified PVC resin, (3)regularly cleaning drying system, (4)regularly replacing air filter cotton.
出处
《聚氯乙烯》
CAS
2016年第1期14-16,共3页
Polyvinyl Chloride
关键词
PVC
旋风干燥器
杂质粒子数
挥发物质量分数
影响因素
措施
PVC
cyclone dryer
impurity particle number
volatile matter mass fraction
influencing factor
measure