期刊文献+

Effect of Wafer Size on the Film Internal Stress Measurement by Wafer Curvature Method 被引量:1

Effect of Wafer Size on the Film Internal Stress Measurement by Wafer Curvature Method
下载PDF
导出
摘要 Wafer curvature method has been applied to determine the internal stress in the films using Stoney's equation.During the film deposition,the wafer fixation on the sample holder will restrict the deformation of the rectangle-shaped wafer,which may result in the stress datum difference along length and width direction.In this paper,the effect of wafer size and the wafer fixation on the TiN film internal stress measured by wafer curvature method was discussed.The rectangle-shaped wafers with different length/width ratios(L/W=1:1,2:1,3:1 and 4:1) were fixed as a cantilever beam.After the TiN films deposition,the profiles of the film/wafer were measured using a stylus profilometer and then the internal stress was calculated using the Stoney equation in the film.The results showed that the fixed end of the wafers limited to some degree the curvature of the wafers along the width direction.For film internal stress measured by wafer curvature method,the wafer profile should be scanned along the length direction and the scan distance should be greater than or equal to half of wafer length.When the length/width ratio of the wafer reached 3:1,the wafer curvature and the calculated stress were basically the same at different positions along the length direction.For film internal stress measured by wafer curvature method,it was recommended that the length/width ratio of wafer should be considered to be greater than or equal to 3:1,and the deformed profile was scanned along the length direction. Wafer curvature method has been applied to determine the internal stress in the films using Stoney's equation.During the film deposition,the wafer fixation on the sample holder will restrict the deformation of the rectangle-shaped wafer,which may result in the stress datum difference along length and width direction.In this paper,the effect of wafer size and the wafer fixation on the TiN film internal stress measured by wafer curvature method was discussed.The rectangle-shaped wafers with different length/width ratios(L/W=1:1,2:1,3:1 and 4:1) were fixed as a cantilever beam.After the TiN films deposition,the profiles of the film/wafer were measured using a stylus profilometer and then the internal stress was calculated using the Stoney equation in the film.The results showed that the fixed end of the wafers limited to some degree the curvature of the wafers along the width direction.For film internal stress measured by wafer curvature method,the wafer profile should be scanned along the length direction and the scan distance should be greater than or equal to half of wafer length.When the length/width ratio of the wafer reached 3:1,the wafer curvature and the calculated stress were basically the same at different positions along the length direction.For film internal stress measured by wafer curvature method,it was recommended that the length/width ratio of wafer should be considered to be greater than or equal to 3:1,and the deformed profile was scanned along the length direction.
出处 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2016年第1期93-99,共7页 武汉理工大学学报(材料科学英文版)
基金 Funded by National Scholastic Athletics Foundotion(NSAF)(No.U1330113) National Natural Science Foundation of China(No.81271953)
关键词 film internal stress wafer curvature method wafer size wafer fixation film internal stress wafer curvature method wafer size wafer fixation
  • 相关文献

参考文献24

  • 1Oettel H, Wiedemaun R, Preifller S. Residual Stresses in Nitride Hard Coatings Prepared by Magnetron Sputtering and Arc Evaporation[J]. Surface and Coatings Technology, 1995, 74-75(1): 273-278.
  • 2Liu D G, Tu J P, Gu C D, et al. Tribological and Mechanical Behaviors of TiN/CNx Multilayer Films Deposited by Magnetron Sputtering[J]. Thin Solid Films, 2011, 519:4 842-4 848.
  • 3Gettel H, Wiedemann R, Residual Stresses in PVD Hard Coatings[J]. Surface and Coatings Technology, 1995, 76-77:265-273.
  • 4Teixeira V. Mechanical Integrity in PVD Coatings due to the Presence of Residual Stresses[J]. Thin Solid Films, 2001, 392:276-28 l.
  • 5Thornton J A, Hoffman D W. Stress-related Effects in Thin Films[J]. Thin Solid Films, 1989, 171 (1): 5-31.
  • 6Richter F, Kupfer H, Schlott P, et al. Optical Properties and Mechanical Stress in SiO2/Nb205 Multi-layers[J]. Thin Solid Films, 2001, 389 (1-2): 278-283.
  • 7Vink T J, Walrave W, Daams J L, et aL Stress, Strain and Microstructure in Thin Tungsten Films Deposited by DC Magnetron Sputtering[J]. a Appl. Phys., 1994, 74(2): 988-994.
  • 8Hauk V, Macherauch E. A Useful Guide for X-ray Stress Evaluation[J]. Adv. X-ray Analysis, 1984, 7:81-99.
  • 9Ma C H, Huang J H, Chen H. Residual Stress Measurement in Textured Thin Film by Grazing Incidence X-ray Diffraction[J]. Thin Solid Film, 2002, 418(2):73-78.
  • 10Verghese P M, Clarke D R. Piezoelectric Contributions to the Electrical Behavior of ZnO Varistors[J]. J. Appl. Phys., 2000, 87:4 430-4 438.

同被引文献6