摘要
在云南晋宁细粒级磷矿浮选中加入600g/t原矿的选择性絮凝剂,经过2min的浮选搅拌,浮选指标得到较大提高,说明选择性絮凝浮选是细粒浮选的一种有效方法。
Selective flocculant was added in 600g/t crude ore in the flotation of fine-grained fraction cellophane in Jinning and stirred for 2minutes with the significant improvement in the flotation index,which indicates flotation with the selective flocculant is an effective method for flotation of fine-grained fraction cellophane.
出处
《化工矿物与加工》
CAS
北大核心
2016年第5期18-19,共2页
Industrial Minerals & Processing
关键词
选择性絮凝
胶磷矿
细粒级浮选
selective flocculant
cellophane
fine-grained fraction