摘要
通过试验,从粉磨时间、煅烧温度、激发剂三方面,分析了影响废弃混凝土粉体活化的因素,得到了一些有意义的结论,有利于合理使用废弃混凝土再生粉体,实现建筑垃圾零排放目标。
According to the tests, the paper analyzes the factors influencing the activation of the waste concrete powder from the grinding time,calcinations temperature, and activator, and achieves come meaningful conclusion, so as to apply the recycled powder of the waste concrete reasonably,and realize the zero-emission of architectural rubbish.
出处
《山西建筑》
2016年第15期114-116,共3页
Shanxi Architecture
关键词
废弃混凝土
再生粉体
煅烧温度
抗压强度
waste concrete, recycled powder, calcinations temperature, compressive strength