摘要
针对热轧带钢尾部红褐色柳叶状氧化铁皮缺陷,分析了缺陷形貌特征及分布规律,经过现场试验跟踪,确定了缺陷产生来源,采取了相应的控制措施,该缺陷得到消除。
This article aims at the defects of the red brown willow shaped iron oxide in the tail of the hot rolling strip , The morphology characteristics and distribution of defeets are analyzed. After field lest tracking.identify the source of defects, he corresponding eontrol measures are taken.The defect is eliminated.
出处
《甘肃冶金》
2016年第6期34-37,共4页
Gansu Metallurgy
关键词
氧化铁皮缺陷
红褐色柳叶状
除鳞效果
iron oxide defect
the red brown willow shaped
scale removal effect