Transverse Bending Characteristics in U-channel Forming of Tailor Rolled Blank 被引量:3

Transverse Bending Characteristics in U-channel Forming of Tailor Rolled Blank
原文传递
导出
摘要 Research on the formability of tailor rolled blank (TRB) is of good practical significance and application value because of the enormous potential of TRB in the aspect of automobile lightweight. However, the forming of TRB is problematic because of the varying properties; especially, springback is a main challenge. The transverse bending (bending axis is perpendicular to the rolling direction) of TRB U channel was studied through simulation and experiment. The forming characteristics of TRB U channel during transverse bending were analyzed. The mechanisms of forming defects, including bending springback and thickness transition zone (TTZ) movement, were revealed. On this basis, effects of blank geometric parameters on springbaek and TTZ movement were discussed. The results indicate that springback and TTZ movement happen during transverse bending of TRB U-channel. Nonuni form stress distribution is the most fundamental reason for the occurrence of springback of TRB during transverse bending. Annealing can eliminate nonuniform stress distribution, and thus diminish springbaek of TRB, especially springback on the thinner side. Therefore, springback of the whole TRB becomes more uniform. However, annealing can increase the TTZ movement. Blank thickness and TTZ position are the main factors affecting the formability of TRB U-channel during transverse bending. Research on the formability of tailor rolled blank (TRB) is of good practical significance and application value because of the enormous potential of TRB in the aspect of automobile lightweight. However, the forming of TRB is problematic because of the varying properties; especially, springback is a main challenge. The transverse bending (bending axis is perpendicular to the rolling direction) of TRB U channel was studied through simulation and experiment. The forming characteristics of TRB U channel during transverse bending were analyzed. The mechanisms of forming defects, including bending springback and thickness transition zone (TTZ) movement, were revealed. On this basis, effects of blank geometric parameters on springbaek and TTZ movement were discussed. The results indicate that springback and TTZ movement happen during transverse bending of TRB U-channel. Nonuni form stress distribution is the most fundamental reason for the occurrence of springback of TRB during transverse bending. Annealing can eliminate nonuniform stress distribution, and thus diminish springbaek of TRB, especially springback on the thinner side. Therefore, springback of the whole TRB becomes more uniform. However, annealing can increase the TTZ movement. Blank thickness and TTZ position are the main factors affecting the formability of TRB U-channel during transverse bending.
出处 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2016年第12期1249-1254,共6页
基金 Item Sponsored by National Natural Science Foundation of China(51475086) Natural Science Foundation of Hebei Province of China(E2016501118,E2015501073) China Postdoctoral Science Foundation(2016M591404)
关键词 tailor rolled blank transverse bending springback U-CHANNEL annealing thickness transition zone tailor rolled blank transverse bending springback U-channel annealing thickness transition zone