摘要 某船用辅冷凝器B30合金管发生了大面积早期失效。通过失效B30合金管的腐蚀形貌、腐蚀产物及极化曲线分析其失效原因。结果表明:B30合金管发生了选择性腐蚀,其内表面局部区域发生的严重腐蚀是由点蚀引起的脱镍腐蚀,点蚀坑内的酸化环境使脱镍腐蚀更加严重;由于铜的电位正于镍的,铜在晶粒边界附近发生回沉积。 Early failure happened in large areas of B30 alloy tube used for vessel auxiliary condenser. The failure reasons were analyzed through corrosion morphology, corrosion products and polarization curves. The results indicate that selective corrosion happened to B30 alloy, and the most serious corrosion in local area of inner surface was denickel corrosion because of pitting. The acidic environment in the pitting pits made de-nickel corrosion more serious. Potential of copper is more positive than that of nickel, so copper could deposited on grain boundaries.
出处 《腐蚀与防护》 CAS 北大核心 2017年第2期151-154,159,共5页 Corrosion & Protection
关键词 B30合金 脱镍腐蚀 冷凝器 1330 alloy de-nickel corrosion condenser
  • 相关文献

参考文献10

二级参考文献100

共引文献92

同被引文献28

引证文献2

二级引证文献6

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部