摘要
通过计算,确定了设计目标强度为5 MPa,10 MPa和15 MPa的低强度再生碎砖混凝土的配合比,并将再生混凝土制作成多孔砖,通过试验得出了低强再生碎砖混凝土多孔砖的抗压强度,其满足实际工程的需要。
According calculating, abandoned brick is made into recycled concrete, which design strength is 5 MPa , 10 MPa and 15 MPa . Recy-cled concrete is made into porous brick. Base on the compressive strength experiment, it gets the compressive strength of recycled concrete por-ous brick, meet demand of engineering.
出处
《山西建筑》
2017年第4期132-133,共2页
Shanxi Architecture
基金
2016年度广西区级创新创业教育示范专业建设项目
关键词
低强再生碎砖混凝土
多孔砖
抗压强度
配合比
low-strength recycled cracked bricks concrete, porous brick, compressive strength, proportion