以碘量法及ICP-AES法补正滤液中的残余量共同测定粗碲中的铜量,考察了杂质含量、酸分解试验、沉淀剂分离方法选择、滴定过程中缓冲溶液用量、共存离子等对测定的影响,结果表明:选择合适的酸分解方法,优化各条件参数,测定结果的相对标准偏差(RSD值)在0.15%~0.71%,加标回收率在99.70%~100.26%,精密度好、准确性高,方法简单快速。
The copper volume in crude tellurium is determined by both iodimetry and ICP - AES method that correction of the residual volume of filtrate, the following items are investigated, including impurites content, acid decomposition test, the selection of precipi- tant separation method, the dosage of buffer solution in the titration process, the effect of co-existing ion on determination, the results show: the proper acid decomposition method is selected, and each parameters are optimized, the relative standard deviation (RSD) of determining results is in the range of 0. 15% -0. 71%, the recovery rate with standard is in 99.70% - 100. 26%, which has good precision, high accu- racy, the method is simple and rapid.
出处
《云南冶金》
2017年第3期55-61,共7页
Yunnan Metallurgy
基金
工信厅科[2016]58号(项目编号:2016-0216T-YS)
自治区直属公益性科研院所基本科研业务费专项(项目编号:2015ACZ05)
关键词
碘量法
ICP-AES法
粗碲
铜量
iodimetry
ICP- AES method
crude tellurium
copper volume