摘要 The effect of mineralogy and texture on the beneficiation of goethitic ores from two different origins is highlighted. Sample A having 54.47% Fe with 8.57% loss of ignition (LOl) indicates the presence of vitreous and ochreous goethite, martite and microplaty hematite as the major minerals. Sample B contains 56.90% Fe with 14.4% LOI. There is a pisolithic laterite containing vitreous and ochreous goethite, quartz, kaolinitic clay and there is no hematite mineral. The liberated minerals in -150 + 100 μm size class are 74% for Sample A and 37% only for Sample B which shows that the Sample A appears to be more amenable to beneficiate. A concentrate of 46.7% with 63.22% Fe could be recovered from Sample A while subjected to gravity separation followed by wet magnetic separation. The Sample B does not respond to gravity and magnetic separation due to its complex mineralogy. However, calcination of the Sample B followed by magnetic separation gives the encouraging results. Thus, anomalous behaviour of the goethite dominated ores in beneficiation is attributed to the different textural and liberation characteristic. The effect of mineralogy and texture on the beneficiation of goethitic ores from two different origins is highlighted. Sample A having 54.47% Fe with 8.57% loss of ignition(LOI) indicates the presence of vitreous and ochreous goethite, martite and microplaty hematite as the major minerals. Sample B contains 56.90% Fe with 14.4% LOI. There is a pisolithic laterite containing vitreous and ochreous goethite, quartz, kaolinitic clay and there is no hematite mineral. The liberated minerals in -150 + 100μm size class are 74% for Sample A and 37% only for Sample B which shows that the Sample A appears to be more amenable to beneficiate. A concentrate of 46.7% with 63.22% Fe could be recovered from Sample A while subjected to gravity separation followed by wet magnetic separation. The Sample B does not respond to gravity and magnetic separation due to its complex mineralogy. However, calcination of the Sample B followed by magnetic separation gives the encouraging results. Thus, anomalous behaviour of the goethite dominated ores in beneficiation is attributed to the different textural and liberation characteristic.
出处 《International Journal of Mining Science and Technology》 SCIE EI CSCD 2017年第3期445-450,共6页 矿业科学技术学报(英文版)
基金 Ministry of Steel for funding the research work (GAP 0224)
关键词 Texture Pisolitic Ochreous goethite Vitreous goethite Calcination 选矿过程 矿物学 织构 针铁矿 高岭石粘土 赤铁矿 湿式磁选 重力分离
  • 相关文献

参考文献2

二级参考文献10

共引文献38

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部