摘要
二氧化钼是由三氧化钼生产钼粉过程中的中间产品,调整二氧化钼粒度是控制钼粉粒度的重要手段。通过对生产进行跟踪,研究了三氧化钼原料粒度、料层厚度、还原温度、氢气露点等因素对二氧化钼粒度的影响规律。
MoO2 are the intermediate products in the processing of MoO3 to Mo powders. It is very important to adjust the size of MoO2 in order to control the particle size of Mo powder. In this paper,affecting factors such as initial MoO3 particle size,layer thickness,reduction temperature and hydrogen gas dew point were studied during the procedure tracking.
出处
《矿冶》
CAS
2017年第5期62-64,共3页
Mining And Metallurgy
关键词
一段还原
二氧化钼
粒度
one-stage reduction
MoO2
particle sizes