文章分析了贵溪冶炼厂2#闪速炉包底铜产出的原因,通过对炉况波动影响的调整、定期洗炉、作用方式的变化、渣口直径的变化,包底铜的产出量由475 t/月降至158 t/月。
This paper analyzes the causes of bottom copper output in the 2#furnace in Guixi smelter. Through changing the influence of furnace condition fluctuation adjustment,regular washing,changing the mode of action of furnace,slag hole diameter,the output of copper ladle is reduced from 475 t/m to 158 t/m.
出处
《湖南有色金属》
CAS
2017年第5期37-39,共3页
Hunan Nonferrous Metals
关键词
包底铜
闪速炉
沉淀池
渣口水套
ladle base copper
flash furnace
sedimentation tank