摘要
为研究9.5~16 mm粒径范围内的再生粗骨料干燥和潮湿两种状态对再生混凝土的力学性能影响,以干燥状态再生粗骨料作为对比进行干湿两种状态再生粗骨料替代率为0、20%、40%、60%、80%、100%等质量替代天然粗骨料配制6种C30混凝土,对不同状态下的再生混凝土进行抗压和劈裂拉伸试验。结果表明:潮湿状态下的再生粗骨料对应的再生混凝土抗压和劈裂拉伸强度均低于干燥状态下再生粗骨料对应的再生混凝土抗压和劈裂拉伸强度。
It mainly aimed at studying the effect of dry and wet recycled coarse aggregate on the mechanical properties of recycled concrete between 9.5-16 mm diameter range.It compared the dry state with dry and wet state of recycled coarse aggregate, which compounded 6 kinds of C30 concrete with same quality of natural aggregate under the replacement rate of 0,20%, 40%, 60%, 80%, 100%.Within the process, the compressive strength and splitting tensile strength were tested.Results showed that both of the compressive strength and splitting tensile strength of wet recycled coarse aggregate were lower than those of dry recycled coarse aggregate.
出处
《混凝土》
CAS
北大核心
2018年第1期88-90,95,共4页
Concrete
基金
国家自然科学基金资助项目(11162015)
宁夏回族自治区服务地方经济项目(NGY2016236)
宁夏回族自治区大学生创新试验项目(20150152)
关键词
再生粗骨料
再生混凝土
干湿状态
抗压强度
劈裂拉伸强度
recycled coarse aggregate
recycled concrete
dry and wet state
compressive strength
splitting tensile strength