摘要
在保持原有铜钼混合浮选-铜钼分离浮选工艺的基础上,采用多种新型捕收剂、抑制剂分别对云南某斑岩型铜钼矿混合浮选、铜钼分离浮选进行了药剂优化试验研究,最终选用捕收剂W3和W4、起泡剂F-425和MIBC、高效的铜抑制剂M8等,并进行全流程闭路试验,获得了钼品位44.92%、钼回收率80.57%的钼精矿,铜品位25.03%、铜回收率91.10%的铜精矿。与设计流程浮选指标相比,铜回收率提高了回收率提高了4.10个百分点,钼的回收率提高了4.57个百分点。
Without changing the original copper-molybdenum mixed flotation and copper-molybdenum separation process,a variety of new collectors and inhibitors are used to study the reagent system optimization for a copper-molybdenum mixed flotation and copper-molybdenum separation flotation for a porphyry copper-molybdenum in Yunnan province.The effects of W3 and W4,foaming agent F-425 and MIBC and high-efficiency copper inhibitor M8 are obtained.Ultimately,according to the results of the locked-cycle test,the grade of the molybdenum concentrate comes to 44.92% with a Mo-recovery of80.57%;the grade of the copper concentrate comes to 25.03% with a Cu-recovery of 91.10%.Compared with the flotation index of the design process,the recovery of copper was increased by 4.10 percentage points,and the recovery of molybdenum was increased by 4.57 percentage points.
出处
《中国矿业》
北大核心
2018年第3期132-137,共6页
China Mining Magazine
关键词
铜钼矿
铜钼混浮
铜钼分离
药剂制度
copper-molybdenum ore
copper-molybdenum mixed flotation
copper-molybdenum separation
reagent system