摘要
HXA7-7定向井在固井过程中发生套管泄漏失效事故。采用体积法进行迟到时间试验,并对套管柱进行测井检查,分析了该定向井套管泄漏的原因。结果表明:HXA7-7定向井套管存在原始缺陷,在固井过程中原始缺陷扩展并穿透井壁,最终导致套管泄漏。
Casing leakage occurred during the cementing process of HXA7-7 directional well.Causes analysis of casing leakage in the directional well were analyzed by late time test of volume method,and the casing string was checked by logging.The results show that the original defects in the HXA7-7 directional well casing.In the process of cementing,the original defects spread through the wellbore and eventually lead to the leakage of the casing.
作者
滕学清
杨向同
吕拴录
郭洪志
谢俊峰
耿海龙
李宁
盛勇
秦宏德
雷军
TENG Xueqing;YANG Xiangtong;L Shuanlu;GUO Hongzhi;XIE Junfeng;GENG Hailong;LI Ning;SHENG Yong;QIN Hongde;LEI Jun;(1. Tarim Oilfield, Kuerle 841000, China 2. Department of Materials, Eleetromechanic Engineering College, China University of Petroleum, Beijing 102249, China; 3. Schlumberger, Beijing 100015, Chin)
出处
《理化检验(物理分册)》
CAS
2018年第3期195-197,共3页
Physical Testing and Chemical Analysis(Part A:Physical Testing)
关键词
固井
套管
泄漏
测井
cementing
casing
leakage
well logging