High mercury leachate containing HgS22- complex ion: Detoxifying solidification and high efficiency Hg extraction

High mercury leachate containing HgS_2^(2-) complex ion:Detoxifying solidification and high efficiency Hg extraction
原文传递
导出
摘要 Clean and efficient treatment of high-mercury leachate produced from remediation of mercury-polluted soil has become a huge challenge for environmental scientists. In this work, cement solidification was firstly adopted to treat the high-concentration mercury leachate, which had high alkalinity. Different mercury concentrations, namely 3.120 mg/L Hg mercury leachate and 9.243 mg/L Hg mercury concentrated leachate, were separately solidified by Portland cement. The results indicated that simply using the cement can properly solidify both the leachates to meet the waste landfill standard, with liquid (mL)/solid (g) ratio (US ratio) of 4:10-6:10. In order to make full use of mercury in the leachates, a Hg extraction method was subsequently carried out under different experimental parameters, such as temperature and pH value. It was shown that the Hg extraction ratio could reach as high as 99.84% and almost all the mercury in the leachate could be transformed to HgS precipitate; moreover, the Hg concentration in the treated leachate was reduced from 3.120 to 0.005 mg/L at pH 2.98 and 30℃, which was much less than the limit of the national standard, indicating that the leachate had been completely cleaned and could be discharged freely. Hence, simple cement solidification renders high-mercury leachate nontoxic, and the Hg extraction method can successfully recover the Hg and enable the residual leachate to be discharged safely. Clean and efficient treatment of high-mercury leachate produced from remediation of mercury-polluted soil has become a huge challenge for environmental scientists. In this work, cement solidification was firstly adopted to treat the high-concentration mercury leachate, which had high alkalinity. Different mercury concentrations, namely 3.120 mg/L Hg mercury leachate and 9.243 mg/L Hg mercury concentrated leachate, were separately solidified by Portland cement. The results indicated that simply using the cement can properly solidify both the leachates to meet the waste landfill standard, with liquid (mL)/solid (g) ratio (US ratio) of 4:10-6:10. In order to make full use of mercury in the leachates, a Hg extraction method was subsequently carried out under different experimental parameters, such as temperature and pH value. It was shown that the Hg extraction ratio could reach as high as 99.84% and almost all the mercury in the leachate could be transformed to HgS precipitate; moreover, the Hg concentration in the treated leachate was reduced from 3.120 to 0.005 mg/L at pH 2.98 and 30℃, which was much less than the limit of the national standard, indicating that the leachate had been completely cleaned and could be discharged freely. Hence, simple cement solidification renders high-mercury leachate nontoxic, and the Hg extraction method can successfully recover the Hg and enable the residual leachate to be discharged safely.
出处 《Journal of Environmental Sciences》 SCIE EI CAS CSCD 2018年第11期177-184,共8页 环境科学学报(英文版)
基金 supported by the National Natural Science Foundation of China(Nos.51672025,51572020,51372019) Major Projects of Science and Technology in Shanxi Province(No.MC2016-03)
关键词 High mercury leachate Cement solidification Mercury extraction Cleaning and efficiency High mercury leachate Cement solidification Mercury extraction Cleaning and efficiency