摘要 剖析了苯乙烯装置原进口乙苯 /蒸汽过热器的失效原因 ,并提出了解决问题的技术措施 ,即通过合理选材避免了材质的高温回火脆化 ;改进滑动管板结构 ,使滑动管板易于滑动。 In this paper the factors causing the failure of the imported ethylbenzene/steam superheater in styrene plant of Qilu Petrochemical Corp.are analysed and the quick fix is proposed.The high temperature temper embrittlement was prevented by a rational material selection and the stress in the tube sheet was considerablely reduced by improving its design for ease to slide.The commercial pratice proved the improvements successful.
作者 乔学福
出处 《化工进展》 EI CAS CSCD 北大核心 2002年第9期685-688,共4页 Chemical Industry and Engineering Progress
关键词 乙苯 蒸汽过热器 失效原因 改进措施 苯乙烯装置 回火脆化 ethylbenzene/steam superheater, invalidation, measure,backfire brittle
  • 相关文献

同被引文献16

  • 1苏杨.乙苯蒸发过热器的设计[J].石油化工设备,1995,24(5):33-36. 被引量:2
  • 2田春霞,仇性启,张兵,马培勇.苯乙烯装置过热器组支座受力分析[J].石油化工设备,2006,35(1):48-50. 被引量:5
  • 3李永泰.EA304换热器管板应力分析计算.第二届全国换热器学术会议论文集.合肥:压力容器杂志社,2001.51-55
  • 4王正方,徐桂根,刘敏.乙苯蒸汽过热器管板的制造.第二届全国换热器学术会议论文集.合肥:压力容器杂志社,2001.82-85
  • 5崔流芳,王新民,石象增等.管孔应力槽加工装置.中国专利,CN98221958.1.1998.8.18
  • 6崔流芳,王新民,石象增等.一种加工槽的工具.中国专利,CN98221960.1.1999.6.26
  • 7崔培祥,薛兆军,武朋建等.管子管板内孔自动焊焊枪及枪头.中国专利,CN98222570.9.1999.12.15
  • 8李永泰.EA304换热器管板应力分析计算[A].第二届全国换热器学术会议论文集[C].合肥:压力容器杂志社,2001.11,51-55.
  • 9王正方,徐桂根,刘敏.乙苯蒸汽过热器管板的制造[A].第二届全国换热器学术会议论文集[C].合肥:压力容器杂志社,2001.11,82-85.
  • 10宋永兰.EA-304乙苯/蒸汽过热器断裂管束的修复再利用[J].化工机械,1998,25(2):102-103. 被引量:2

引证文献2

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部