一、前言钨制品的深度加工,要求有高质量的钨粉。运用电子计算机控制钨粉生产,不仅可以保证产品质量和提高劳动生产率,而且可以得到预期产品和再现性。通过微机控制蓝钨五段还原炉的温度、氢气流量、推舟速度等三个主要还原参量,达到了稳定生产的目的。为了获得合格的 W31钨粉,必须在此基础上寻找最佳工艺条件。W31钨粉的生产取决于工艺条件和原料的性质。各批原料的性质可能存在着波动,因此每批原料应该进行试探实验,寻找该批料还原生产 W31钨粉的最佳工艺条件。W31钨粉是由 W31D 粉和 W31B 粉混合而成,W31B 粉的工艺条件不宜改变,所以必须对 W31D 粉生产的工艺条件进行研究。本实验就是利用微机控制系统,寻找蓝钨还原制取 W31D 粉的最佳工艺条件。
The effect of various process parameters on the particle size of tungs- ten powder in the reduction of blue tungsten oxide into tungsten by hydrogen has been studied in this paper.The optimal process conditions for producing tungsten powder from blue tungsten oxide has been found through an orthogonal experiment on an industrial scale.The experimental data were processed with a computer and a quadratic regression equation was established for predcting and controlling the particle size of tungsten powder.