摘要 对SL(钢包喷吹Ca-Si粉 )工艺和CAB(钢包吹氩 )工艺轴承钢GCr15的K1c和ΔKth进行了测定 ,并对裂纹失稳扩展的临界尺寸和亚稳扩展的起始尺寸进行了估算。结果表明 :采用SL工艺的GCr15钢K1c和ΔKth均有所提高 ;裂纹失稳扩展和临界尺寸和亚稳扩展的起始尺寸是CAB工艺的 2倍。 The K 1c and ΔK th of bearing steel GCr15 by SL and CAB processing were measured.The critical dimension of crack quick propagating and the initial dimension of crack sub-propagating were estimated.The results show that the K 1c and ΔK th of steel GCr15 can be improved by SL technology.The critical dimension of cracks quick propagating and the initial dimension of cracks sub-propagating of SL technology are double times than CAB technology.
机构地区 鸡西大学
出处 《煤炭技术》 CAS 2002年第9期58-59,共2页 Coal Technology
关键词 喷吹工艺 GCR15轴承钢 裂纹尺寸 裂纹失稳扩展 力学性能 钢包吹氩工艺 processing of SL and CAB GCr15 steel K 1c and ΔK th crack size
  • 相关文献

参考文献1

二级参考文献1

  • 1[苏]斯别克托尔(А·Г·Спектор)等 著,本溪钢铁公司一钢厂,抚顺钢厂.轴承钢的组织与性能[M]上海科学技术文献出版社,1983.

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部