摘要 某含磷磁铁矿石中磷和铁的品位都很低 ,且磁性铁矿物含量只占总铁的 60 %。矿石经磁滑轮预选可抛除 1/3的尾矿 ,预选粗精矿磨至 -0 0 74mm占 60 % ,经浮选可获得含P2 O53 7 2 8%的磷精矿。选磷尾矿通过磁选粗选、磁粗精矿再磨后磁选精选 ,可获得含铁为 65 2 1%的铁精矿 ,磁性铁回收率对原矿中磁性铁为 85 3 9% ,对磁滑轮预选粗精矿中磁性铁为 94 5 6%。 Study on treating low grade magnetic iron ores containing apatite carried out Run of mine was treated with magnetic pulley and non magnetic product(33% yield) went into tailings The preconcentrated rougher magne tic concentrate was ground to 60%-0 074mm,and treated with flotation to obtain phosporus concentrate(37 28% P 2O 5) Then flotation tailings were treated in rougher magnegic separation,then the routher magnetic concentrate was reground and treated in cleaner magnetic separation to obtain iron concentrate(65 21% Fe)
出处 《矿冶》 CAS 2002年第3期35-38,21,共5页 Mining And Metallurgy
关键词 磁铁矿 磷灰石 预选 浮选 磁选 再磨 尾矿 Low grade magnetite Apatite Preconcentration Flotation Magnetic separation Regrinding
  • 相关文献

参考文献3

  • 1朱俊士.中国钒钛磁铁矿选矿[M].北京:冶金工业出版社,1995.294-298.
  • 2胡为柏.浮选[M].北京:冶金工业出版社,1993..
  • 3北京矿冶研究总院.小张家口钒钛磁铁矿小型选矿试验报告[M].,2001..

共引文献1

同被引文献38

引证文献2

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部