摘要
以电解MnO_2(EMD)工业的锰矿渣和高岭土为原料,工业水玻璃为碱激发剂在较低温度下发泡制备锰矿渣地聚物基泡沫材料。单因素实验考察了发泡温度、水玻璃模数、粉体加入量、掺水量等因素对材料的影响。
Manganese slag geopolymer foams were prepared by using manganese slag and kaolin from electrolysis MnO2(EMD)industry as raw materials,and industrial water glass as base activator foaming at lower temperature.Single-factor experiments investigated the effects of foaming temperature,water glass modulus,powder addition,and water incorporation on the material.
作者
周树年
黄连金
王强
ZHOU Shu-nian;HUANG Lian-jin;WANG Qiang(Guangxi Normal University for Nationalities,Guangxi Chongzuo 532200,China)
出处
《科技视界》
2018年第5期20-21,共2页
Science & Technology Vision
基金
2013年度广西民族师范学院校级自然科学研究立项项目(2013YB012)
关键词
锰矿渣
地聚物
碱激发
多孔材料
Manganese slag
Geopolymers
Alkali excitation
Porous materials