摘要
云南某含银铜矿石银品位为21.77 g/t,主要赋存于黄铜矿、游离银和磁黄铁矿中,在选别过程中铜硫分离时兼顾银的回收具有一定的难度。采用抑硫浮铜流程,研究筛选出石灰及Z200作为合适的调整剂和高效捕收剂,在抑制黄铁矿、磁黄铁矿的同时强化银的回收。最终闭路试验获得了品位23.92%、回收率97.10%的铜精矿,且含银136.38 g/t,银的回收率达到77.05%,实现了铜硫分离的同时强化银的回收。
A silver-bearing copper ore in Yunnan occurs mainly in the form of chalcopyrite free silver and pyrrhotite,with a silver grade of 21.77 g/t.In the process of beneficiation,it is difficult to recover associated silver effectively while Cu and S are being separated.To solve this problem,an enhanced recovery process of inhibiting sulfur-floating copper was tested,and lime and Z200 were used as both the regulator and collector.After a closed circuit test,copper was concentrated to a grade of 23.92%with a recovery of 97.10%while the content of silver was simultaneously upgraded to136.38 g/t with a recovery of 77.05%,indicating that the separation of copper and sulfur had been realized and the recovery of silver was simultaneously strengthened.
作者
宋宝旭
邱显扬
胡佛明
李沛伦
邹坚坚
付华
SONG Baoxu;QIU Xianyang;HU Foming;LI Peilun;ZOU Jianjian;FU Hua(Guangdong Institute of Resources Comprehensive Utilization,State Key Laboratory of Rare Metals Separation and Comprehensive Utilization,Guangdong Provincial Key Laboratory of Development and Comprehensive Utilization of Mineral Resource,Guangzhou 510651,China)
出处
《贵金属》
CAS
CSCD
北大核心
2018年第3期47-50,58,共5页
Precious Metals
基金
广州市科技计划项目(20170702005)、广东省科学院实施创新驱动发展能力建设专项(2017GDASCX-0301、2017GDASCX-0839)。
关键词
有色金属冶金
游离银
黄铜矿
抑硫浮铜
磁黄铁矿
强化
nonferrous metallurgy
free silver
chalcopyrite
inhibition sulfur and flotation copper
pyrrhotite
strengthening