摘要
通过理论计算的方法得到镁渣的热容为0.754 J/(g·℃),再采用差示扫描量热法(DSC),以刚玉为标准物质测定了镁渣从常温至700℃的热容数据,并通过回归分析得到了常温至700℃热容与温度的关系式,实验结果与理论计算值基本吻合。
The thermal capacity of magnesium slag is 0.754 J/(g·℃)by theoretical calculation method.Differential scanning calorimetry(DSC)is used to determine the magnesium slag use corundum as the standard material.The heat capacity data from room temperature to 700℃,and the relationship between heat capacity and temperature from room temperature to 700℃were obtained by regression analysis.The experimental results were basically consistent with the theoretical calculations.