摘要
介绍尿素合成塔不锈钢衬里腐蚀减薄严重情况,简要阐述腐蚀的原因,采取一次性全部更换的方法进行改造,详细介绍衬里更换实施过程,改造后运行情况良好。
Serious corrosion happened on stainless steel lining of urea reactor, making the thickness of lining become thinner. The reason of corrosion was briefly described. The reformation of one-time replacement of urea reactor lining was taken. This paper introduced the replacement process in detail and the result after reformation.
作者
但天福
杨嵎森
Dan Tianfu;Yang Yusen(China Blue Chemical Ltd.,Dongfang 572600)
出处
《大氮肥》
CAS
2019年第2期119-121,共3页
Large Scale Nitrogenous Fertilizer Industry
关键词
尿素合成塔
不锈钢衬里
腐蚀减薄
urea reactor
stainless steel lining
corrosion and become thinner