中棒线圆钢表面划伤缺陷改善攻关 被引量:4

Improvement for Scratch Defect on the Medium-size Bar Production Line
下载PDF
导出
摘要 分析了韶钢优特钢中棒线圆钢表面划伤产生的原因,通过对空过辊道进行优化,增加弱穿水工艺,在穿水管入口加装导卫以及改造冷床裙板等措施,有效解决了中棒线圆钢表面划伤问题,显著提升了成品表面质量。 The reason for scratch defect on the medium-size bar production line at SISG is analyzed. The problem is effectively solved with measures: optimizing the empty roller table,adding slight through water cooling process,installing a guide at the entrance of the through water cooling pipe and remodeling the braking skirt plate of cooling bed. The surface quality of products is improved obviously.
作者 张宝华 周小兵 李学保 Zhang Baohua;Zhou Xiaobing;Li Xuebao(Guangdong Shaogang Songshan Co.,Ltd.,Guangzhou Guangdong 510160)
出处 《山西冶金》 CAS 2019年第1期131-133,共3页 Shanxi Metallurgy
关键词 划伤 辊道 弱穿水 冷床裙板 scratch defect roller track slight through water cooling braking skirt plate of cooling bed
  • 相关文献

参考文献2

二级参考文献1

  • 1宋余九 荀毓闽.热处理手册(第2版第4卷).热处理质量控制与检验方法[M].北京:机械工业出版社,1992.212-214.

共引文献2

同被引文献19

引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部