摘要 The physicochemical properties and creepage discharge characteristics of aged high temperature Vulca nized(HTV)silicone rubber materials were investigated by ultraviolet radiati on(UV)aging method in this study.The experimental results show that as the aging time increases,the creepage discharge flashover voltage increases first and then decreases.But the aging time has little effect on the creepage discharge inception voltage.With the aging time prolonged,the discharge endurance time of HTV silicone rubber is shortened,and the creepage discharge development velocity is accelerated.In the short time of applying voltage to aging material,the magnitude of discharge in creases rapidly.According to the partial discharge characteristic parameters of creepage discharge,the whole creepage discharge process is partitioned into four stages.Compared with unaged HTV silicone rubber,the aged HTV silicone rubber has less fluctuation in performance parameters and a clear trend.The study found that UV aging not only affects the physicochemical and hydrophobic properties of the HTV silicone rubber,but also accelerates the development of creepage discharge under AC voltage. The physicochemical properties and creepage discharge characteristics of aged high temperature Vulcanized(HTV) silicone rubber materials were investigated by ultraviolet radiation(UV)aging method in this study. The experimental results show that as the aging time increases, the creepage discharge flashover voltage increases first and then decreases. But the aging time has little effect on the creepage discharge inception voltage. With the aging time prolonged, the discharge endurance time of HTV silicone rubber is shortened, and the creepage discharge development velocity is accelerated. In the short time of applying voltage to aging material, the magnitude of discharge increases rapidly. According to the partial discharge characteristic parameters of creepage discharge, the whole creepage discharge process is partitioned into four stages. Compared with unaged HTV silicone rubber, the aged HTV silicone rubber has lessfluctuation in performance parameters and a clear trend. The study found that UV aging not only affects the physicochemical and hydrophobic properties of the HTV silicone rubber, but also accelerates the development of creepage discharge under AC voltage.
作者 金福宝 周远翔 梁斌 梁曦东 周仲柳 张灵 Fubao JIN;Yuanxiang ZHOU;Bin LIANG;Xidong LIANG;Zhongliu ZHOU;Ling ZHANG
出处 《Plasma Science and Technology》 SCIE EI CAS CSCD 2019年第5期23-33,共11页 等离子体科学和技术(英文版)
基金 supported by the program for Major Project of the Natural Science Foundation of Qinghai Province(No.2016-ZJ-925Q) Chinese National Programs for Fundamental Research(No.2011CB209400)and(VSN 201602),(2017-K-23)
关键词 HIGH temperature vulcanized silicone rubber CREEPAGE discharge UV AGING INCEPTION VOLTAGE FLASHOVER VOLTAGE HIGH altitude characteristic parameters high temperature vulcanized silicone rubber creepage discharge UV aging inception voltage flashover voltage high altitude characteristic parameters