期刊文献+

2550 m^3高炉炉役后期冷却壁漏水治理及操作优化 被引量:1

Water Leakage Control and Operation Optimization of Water-cooled Panels of Blast Furnace 2550 m^3 in Later Service Period
下载PDF
导出
摘要 南钢2号高炉(2550 m^3)连续生产已近13年,冷却壁漏水严重。对炉役后期的冷却壁破损状况、破损原因、维护措施、漏水治理、高炉操作优化等方面进行了阐述和分析,通过采取一系列冷却壁漏水治理应对措施,实现了炉役后期高炉的安全、高效生产。 The Blast Furnace 2#(2550 m^3)at NISCO has been in continuous production for nearly 13 years, therefore the water leakage of the cooling panels is serious recently. This article describes and analyzes the damage condition, damage reason, maintenance measures, water leakage control and operation optimization of blast furnace in the later service period. By adopting a series of measures for water leakage control of cooling panels, the safe and efficient production of blast furnace in the later service is achieved.
作者 刘永辉 胡正文 LIU Yonghui;HU Zhengwen(Iron-making Plant 1#)
机构地区 第一炼铁厂
出处 《南钢科技与管理》 2019年第2期31-34,共4页 NISCO Technology and Management
关键词 高炉 炉役后期 冷却壁破损 漏水治理 操作优化 Blast Furnace Later Service Period Water-cooled Panel Damage Water Leakage Control Operation Optimization
  • 相关文献

同被引文献3

引证文献1

二级引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部