摘要 Cleaning of high antimony smelting slag from an oxygen-enriched bottom-blown was tested by direct reduction in a laboratory-scale electric furnace.The effects of added CaO,mass ratio of coal(experimental)to coal(theoretical)(ω)and the slag type on the reduction procedure were considered.The contents of Sb and Au were investigated.Iron contamination of the metal phase was analyzed as this may impede the economical viability of this process.The initial slag,coal and CaO were mixed and homogenized before charging into the furnace,and the residual slag averagely contains 1.26 g.ton^-1 Au and1.17 wt% Sb.However,the iron contamination of antimony alloy becomes unacceptably high in this case as the metal phases contain up to 10 wt% Fe.In the slag system with mass ratio of SiO2:FeO:CaO= 45:27:18,the residual slag obtained after reduction under these conditions averagely contains<1 g·ton^-1 Au and<1 wt% Sb,and the metal phase contains<7 wt% Fe.The recoveries of Au in the metal phase are>98 % in all experiments which is proved to be an economic and cleaning process. Cleaning of high antimony smelting slag from an oxygen-enriched bottom-blown was tested by direct reduction in a laboratory-scale electric furnace.The effects of added CaO,mass ratio of coal(experimental)to coal(theoretical)(ω)and the slag type on the reduction procedure were considered.The contents of Sb and Au were investigated.Iron contamination of the metal phase was analyzed as this may impede the economical viability of this process.The initial slag,coal and CaO were mixed and homogenized before charging into the furnace,and the residual slag averagely contains 1.26 g.ton-1 Au and1.17 wt% Sb.However,the iron contamination of antimony alloy becomes unacceptably high in this case as the metal phases contain up to 10 wt% Fe.In the slag system with mass ratio of SiO2:FeO:CaO= 45:27:18,the residual slag obtained after reduction under these conditions averagely contains<1 g·ton-1 Au and<1 wt% Sb,and the metal phase contains<7 wt% Fe.The recoveries of Au in the metal phase are>98 % in all experiments which is proved to be an economic and cleaning process.
出处 《Rare Metals》 SCIE EI CAS CSCD 2019年第8期800-804,共5页 稀有金属(英文版)
基金 financially supported by the National Natural Science Foundation of China(No.51204210) the National High Technology Research and Development Program of China(No.2011AA061001) the National "Twelfth Five-Year" Plan for Science and Technology(No.2012BAC12B04)
关键词 HIGH ANTIMONY SLAG Direct CLEANING reduction Gold High antimony slag Direct cleaning reduction Gold