摘要
通过电化学测量、盐雾试验、周浸试验、机械和疲劳性能测试及应力腐蚀试验,研究了碳纤维环氧复合材料与30CrMnSiA钢的接触腐蚀特性。其结果表明:30CrMnSiA钢与碳纤维环氧复合材料之间存在严重的接触腐蚀,但不影响30CrMnSiA的应力腐蚀性能。文中还给出了防止碳纤维环氧复合材料与30CrMnSiA接触腐蚀的防护措施。
Galvanic corrosion characteristics of graphite epoxy composite materials (GECM) coupled with 30CrMnSiA steel have been studied by electrochemical measurement, salt spray test, alternate-immesion test, performance test and stress corrosion test. Test results show that there is a serious galvanic corrosion between GECM and 30CrMnSiA steel, GECM does not affect the stress corrosion behavior of 30CrMnSiA. The article also gives some galvanic corrosion control methods for couple of GECM and 30CrMnSiA steel.
出处
《材料工程》
EI
CAS
CSCD
北大核心
1992年第5期31-33,39,共4页
Journal of Materials Engineering
关键词
接触腐蚀
碳纤维
复合材料
Galvanic Corrosion, Graphite Epoxy Composite Materials.