摘要
金鼎锌业有限公司南场采选厂处理蜂子山硫化矿时,硫化铅精矿含锌和硫化锌精矿含铅超出设计指标,硫化锌精矿品位较低。研究表明,选厂磨矿细度不够,建议将一段磨矿流程改为两段磨矿流程。
Fengzishan sulphide ore is treated by Nanchang mining plant of Jinding Zinc Industry Co.,Ltd.,the zinc content in lead sulfide concentrate and the lead content in zinc sulfide concentrate exceed the design specifications,the grade of zinc sulfide concentrate is very low.The research show,the grinding fineness of the dressing plant is not enough,it is suggested that the primary grinding flow should be changed to two section grinding flow.
作者
赵树玉
朱从杰
任婷
ZHAO Shu-yu;ZHU Cong-jie;REN Ting(Yunnan Jinding Zinc Industry Co.,Ltd.,Lanping,Yunnan 671400,China;Kunming Metallurgical Research Institute Company Limited,Kunming,Yunnan 650031,China)
出处
《云南冶金》
2020年第1期23-26,共4页
Yunnan Metallurgy
关键词
硫化铅锌矿
浮选
磨矿细度
lead-zinc sulfide ore
flotation
grinding finess