摘要 分析了带肋钢筋横肋末端间隙超出标准的原因,包括加工成品孔型的刀具磨损量太大、轧钢时的轧槽磨损严重等。通过定期更换成品孔型加工刀具、改变轧槽横肋末端的加工方法和及时更换轧槽,使成品带肋钢筋横肋末端间隙尺寸满足热轧带肋钢筋标准GB/T1499.2-2018的要求。 The causes of out-of-standard interval between transverse rib ends of rebar such as excessive wear of machining tool for finish-rolling groove,serious wear of finish-rolling groove in steel rolling process,etc.are analyzed.The interval between transverse rib ends of rebar meets the requirement of GB/T1499.2-2018 hot rolled rebar standard by replacing the machining tool of finish-rolling groove regularly,changing the machining method of transverse rib end in finish-rolling groove,and replacing the finish-rolling groove in time.
作者 李勇 胡友红 王海益 蒙世东 游建 Li Yong;Hu Youhong;Wang Haiyi;Meng Shidong;You Jian(Industrial Department of Steelmaking and Steel Rolling,Shougang Shuicheng Iron&Steel(Group)Co.,Ltd,.Liupanshui 553028,Guizhou,China)
出处 《水钢科技》 2020年第1期19-22,共4页 Shuigang Science & Technology
关键词 带肋钢筋 横肋末端间隙 加工标准 rebar interval between transverse rib ends machining standard
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部