摘要
本研究开展了含金物料高温氯化挥发提金试验,通过控制氯化钙添加初始温度、高温氯化终点温度、氯化钙添加量以及氯化挥发时间,可以使渣中金含量降至0.26 g/t,金的挥发率为98.03%。
In this study,gold-containing materials were subjected to high-temperature chlorination and volatile gold extraction experiments.By controlling the initial temperature of calcium chloride addition,the high-temperature chlorination end temperature,the amount of calcium chloride addition,and the chlorination volatilization time,the gold content in the slag can be reduced to 0.26 g/t,and the gold volatility rate is 98.03%.
作者
张树科
曲邦定
Zhang Shuke;Qu Bangding(Sanmenxia Jinqu Gold and Silver Refining Co.,Ltd.,Sanmenxia 472000,China)
出处
《中国资源综合利用》
2020年第2期8-10,共3页
China Resources Comprehensive Utilization
关键词
含金物料
高温氯化挥发
挥发率
cyanidation residue
high temperature chlorination volatilization
volatilization rate