摘要
本文通过烧结杯试验、矿相分析等手段研究了钒钛烧结矿和普通烧结矿的冶金性能、矿物组成和结构。研究表明,在碱度和燃料配加相同的条件下,钒钛烧结矿和普通烧结矿的还原性指数基本相同,但钒钛烧结矿冷强度和低温还原粉化指数较低,其转鼓指数比普通烧结矿的转鼓指数低12%~18%;低温还原粉化率(RDI+3.15)仅24.92%,比普通烧结矿低50%。烧结矿矿相分析表明,钒钛烧结矿中含20%~23%钙钛矿,矿物分布不均匀,主要以粒状结构和骸晶结构为主。普通烧结矿基本不含钙钛矿,矿物分布较均匀,以交织熔蚀结构为主。
The metallurgical properties,mineral composition and Structure of vanadium-titanium sinter and ordinary sinter were studied by using sinter pot test and mineral phase analysis.The results show that the reducibility index of V-T i sinter is basically the same as that of ordinary sinter under the same basicity and fuel blending conditions,but the cold strength and low-temperature reductive pulverization index of V-T i sinter are lower,the drum index of V-Ti sinter is 12%?18%lower than that of ordinary sinter,and the lowtemperature reductive pulverization rate(RDI+3.15)is only 24.92%,which is 50%lower than that of ordinary sinter.The sinter phase analysis shows that the vanadium-titanium sinter contains 20%?23%perovskite with uneven distribution of minerals,which presents mainly granular structure and skeletal crystal structure.The ordinary sinter basically contains no perovskite,and the distribution of minerals is more uniform.
作者
王自学
冯帅
Wang Zixue;Feng Shuai(HBIS Group Han Steel Company,Han bao iron works,Handan,Hebei,China)
出处
《矿产综合利用》
CAS
北大核心
2020年第1期71-75,共5页
Multipurpose Utilization of Mineral Resources
关键词
钒钛烧结矿
转鼓指数
低温还原粉化率
矿相
Vanadium titanium sinter
Drum index
Reduction disintegration index
Sinter phase