摘要
采用等体积浸渍法制备系列Au/Cu/FLA催化剂,考察了催化剂在干、湿气氛及高浓度CO2气氛下对CO低温氧化的催化能力,并采用N2物理吸脱附、透射电子显微镜、X射线粉末衍射、红外光谱等表征手段对催化剂进行表征.实验结果表明:Au/Cu/FLA系列催化剂都具有较好的初始活性;与干气氛相比,湿气氛下催化剂的稳定性较好;表征结果初步判断引起本系列催化剂失活的可能的主要因素是碳酸盐产生覆盖活性位点与催化剂表面-OH丢失共同作用的结果.
Au/Cu/FLA series catalysts were prepared by the iso-volume method.The relationship between catalyststructrue and initial activity,dry-feed stable,wet-feed stable catalytic performance of catalysts were investigate by BET,TEM X-ray diffraction and Infrared spectrum.The experimental result indicated:The Au/Cu/FLA series catalysts performanced good initial activity;the reaction stability is better in wet atmosphere then dry atmosphere.The main factors that may lead to the inactivation of the catalyst in this series are the results of the joint action of the active site of carbonate production and the loss of-OH.
作者
苏慧娟
郑玉华
孙逊
孙立波
祁彩霞
SU Hui-juan;ZHENG Yu-hua;SUN Xun;SUN Li-bo;QI Cai-xia(Yantai Key Laboratory of Gold Catalysis and Engineering,Shandong Applied Research Center of Gold Nanotechnology(Au-SDARC),School of Chemistry&Chemical Engineering,Yantai University,Yantai 264005,China)
出处
《分子催化》
EI
CAS
CSCD
北大核心
2020年第1期65-71,I0003,共8页
Journal of Molecular Catalysis(China)
基金
国家自然科学基金(21773202)
烟台市重点研发计划(2019LJRC140)。
关键词
CO氧化
纳米金催化剂
反应气氛
CO oxidation
nano-gold catalyst
reactive atmosphere