摘要
分别采用钼酸钠、钼酸铵、磷钼酸、磷钼酸铵合成泡沫镍复合材料,使用XRD和SEM分析合成的泡沫镍复合材料的晶型和形貌.结果表明,泡沫镍复合材料反应最佳条件为:反应温度为200℃,反应时间为10 h.
Foam nickel composite materials were synthesized by ammonium molybdate,ammonium molybdate,molybdate molybdate and ammonium molybdate.The crystal morphology and morphology of the foam nickel composite were analyzed by XRD and SEM.The results showed that the optimum reaction conditions were the reaction temperature was 200℃and the reaction time was 10 h.
作者
陈国力
宋坤
赵楠
王文波
殷广明
黄孝明
CHEN Guoli;SONG Kun;ZHAO Nan;WANG Wenbo;YIN Guangming;HUANG Xiaoming(Teaching and Experimental Equipment Management Center(Engineering Training Center),Qiqihar University,Qiqihar 161006,China)
出处
《高师理科学刊》
2020年第4期66-68,共3页
Journal of Science of Teachers'College and University
基金
黑龙江省省属本科高校基本科研业务费科研项目(135309447)。
关键词
泡沫镍
钼源
XRD
SEM
nickel foam
molybdenum source
XRD
SEM