摘要 研究了冷轧压下率对连退SPCC产品组织和性能的影响。研究结果表明,连退SPCC产品的组织由等轴的铁素体晶粒和晶界处的块状渗碳体及晶粒内的颗粒状渗碳体组成。冷轧压下率越大,晶粒尺寸越小,屈服强度越高。随着冷轧压下率从71%增加至82%,晶粒尺寸减小了5μm,屈服强度增大了33MPa。
出处 《冶金与材料》 2020年第2期65-65,70,共2页 Metallurgy and Materials
关键词
  • 相关文献

参考文献3

二级参考文献14

  • 1WANG Zhao-dong GUO Yan-hui ZHAO Zhong LIU Xiang-hua WANG Guo-dong.Effect of Processing Condition on Texture and Drawability of a Ferritic Rolled and Annealed Interstitial-Free Steel[J].Journal of Iron and Steel Research(International),2006,13(6):60-65. 被引量:4
  • 2付作宝.冷轧薄钢板生产[M].北京:冶金工业出版社,2009:188.
  • 3Juntunen P, Raabe D, Karjalainen P, et al. Optimizing continuous annealing of interstitial-free steels for improving deep drawability [ J ]. Metallurgical and Materials Transactions A, 2001,32 (8) : 1989-1995-.
  • 4Ghosh P, Bhattacharya B, Ray R K. Comparati':e study of precipitation behavior and texture formation in cold rolled-batch annealed and cold rolled-continuous annealed interstitial free high strength steels [ J ]. Scripta Materialia, 2007, 56(8) : 657-660.
  • 5Attallah M M, Strangwood M, Davis C L. Influence of the heating rate on the initiation of primary recrystallization in a deformed A1-Mg alloy [J]. Scfipta Materialia, 2010, 63: 371-374.
  • 6胡庚祥,蔡瑜,戎咏华.材料科学基础[M].上海:上海交通大学出版社,2008.
  • 7D. Daniel,J. J. Jonas. Measurement and prediction of plastic anisotropy in deep-drawing steels[J] 1990,Metallurgical Transactions A(1):331~343
  • 8伍康勉,成小军,陈兴国,周峰.用CSP热轧卷生产的冷轧退火平整板卷的屈服强度问题[J].钢铁,2008,43(5):96-100. 被引量:3
  • 9李萧,杨平,林瑞民,刘西峰,陈冷.低碳钢退火板中粗大晶粒成因的EBSD分析[J].电子显微学报,2009,28(1):34-38. 被引量:10
  • 10张少红,郑志刚,李秀军.SPCC产品的连退工艺研究[J].机械工程与自动化,2010(2):116-118. 被引量:7

共引文献17

同被引文献5

引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部