摘要 This paper clarifies two issues related to the prior cathodic polarisation treatment(PCPT) for the potentiodynamic polarisation test: whether PCPT can(1) remove the air-formed surface film and(2) affect the polarisation test results. X-ray photoelectron spectroscopy analyses of fluoride ion-labelled samples show that PCPT cannot remove the surface film completely due to the low reaction rate. Potentiodynamic polarisation tests demonstrate that PCPT with proper operating parameters,-1.0 V SCE for 5 min with subsequent open circuit potential(OCP) stabilisation in this study, is necessary because it can improve the test reproducibility without affecting the corrosion parameters by unifying the initial surface state. However, PCPT with lower potentials, longer time or no OCP stabilisation has significant effects on the electrochemical corrosion parameters due to the hydrogen absorption under the conditions of this study.
出处 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2020年第6期839-845,共7页 金属学报(英文版)
基金 the National Science and Technology Major Project of China(No.2016ZX05016-004) the National Natural Science Foundation of China(Nos.51801218 and 51571200) the Strategic Priority Research Program of the Chinese Academy of Sciences(No.XDA13040500)。
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部