摘要
非金属材料在油田的应用虽缓解了传统金属材料的腐蚀等问题,但其他方面的失效仍然存在。对塔河油田某计转站HDPE内穿插修复管线开裂失效、某联合站污水外输管线玻璃钢法兰渗漏失效、某单井用塑料合金复合管内衬起泡失效3个典型失效案例进行了系统分析,由此提出了油田用非金属管失效分析与评价体系的基本方法。
Although the application of non-metallic materials in oil field alleviates the corrosion of traditional metal materials,other failures still exist.In this paper,three typical failure cases in Tahe oilfield are analyzed systematically,which are HDPE interpenetrating repair pipeline cracking failure in a transfer station,GFRP flange leakage failure of a combined sewage export pipeline and foaming failure of plastic alloy composite pipe lining used in a well.Therefore,we put forward the basic method of failure analysis and evaluation system of non-metallic pipe used in oil field.
作者
许艳艳
葛鹏莉
肖雯雯
王孟欣
林平林
卿双永
高多龙
刘青山
陈苗
张晓灿
Xu Yanyan;Ge Pengli;Xiao Wenwen;Wang Mengxin;Lin Pinglin;Qing Shuangyong;Gao Duolong;Liu Qingshan;Chen Miao;Zhang Xiaocan(Research Institute of Petroleum Engineering Technology,Sinopec Northwest Oilfield Branch,Urumqi,Xinjiang,China;China University of Petroleum(Beijing),Beijing,China)
出处
《石油与天然气化工》
CAS
CSCD
北大核心
2020年第4期78-82,共5页
Chemical engineering of oil & gas
关键词
塔河油田
非金属管
外层金属爆管失效
法兰失效
脱氯降解失效
失效评价体系
Tahe oilfield
non-metallic tube
failure of outer metal explosion tube
flange failure
dechlorination degradation failure
failure evaluation system