3[1]OHNABE H,Masaki S,Onozuka M,et al.Potential application of ceramic matrix composites to aero-engine components[J].Composites:Part A,1999,30:489-496.
4[3]AKASHI T,TAKESHI N,KOOUN T.Research of CMC application to tube components[J].IHI Engineering Review,2005,38 (2):58-63.
5[4]XU Y D,ZHANG L T,CHENG L F,et al.Microstructure and mechanical properties of three-dimensional carbon/silicon carbide composites fabricated by chemical vapor infiltration[J].Carbon,1998,36 (7-8):1051-1056.
6[5]CHENG L F,XU Y D,ZHANG L T,et al.Oxidation and defect control of CVD SiC coating on three-dimensional C/SiC composites[J].Carbon,2002,40 (12):2229-2234.
7[6]YIN X W,CHENG L F,ZHANG L T,et al.Microstructure and oxidation resistance of carbon/ silicon carbide composites infiltrated with chromium silicide[J].Materials Science and Engineering A,2000,29 (1-2):89-94.
8[7]CHENG L F,XU Y D,ZHANG L T,et al.Effect of glass sealing on the oxidation behavior of three dimensional C/SiC composites in air[J].Carbon,2001,39 (8):1127 -1133.
9[8]WU S J,CHENG L F,ZHANG L T,et al.Oxidation behavior of 2D C/SiC with a multi-layer CVD SiC coating[J].Surface and Coatings Technology,2005,In Press,Available online.
10[9]TSOU H T,KOWBEL W.A hybrid PACVD SiC/CVD-Si3N4/SiC multi-layer coating for oxidation protection of composites[J].Carbon,1995,33 (9):1279-1288.