期刊文献+

实木地板坯料蒸汽干燥垫条痕成因分析及预防措施

Causes Analysis and Preventive Measures of Spacing Strips’Marks on Solid Wood Flooring Blank during Drying Process
下载PDF
导出
摘要 干燥垫条痕是长规格地板坯料干燥过程中容易出现的缺陷之一,坯料初始含水率、干燥环境温度等是产生垫条痕的主要因素,码垛陈放降低坯料入窑前的初始湿度、调整干燥工艺参数、定期检查蒸汽管道排水阀、使用圆方结合体木垫条等是解决地板板面垫条痕缺陷的有效措施。 The spacing strips’mark was one of the defects in the drying process of long-size solid wood flooring blank.The initial moisture content of the blank and the drying environment temperature were the main factors to produce the spacing strips’mark.Reducing the initial moisture content of the blank before entering the kiln,adjusting the drying process parameters,regularly checking the steam pipe drain valve,and using the wood strip with the combination of round and square were the effective preventive measures for spacing strips’mark defects.
作者 田瑞良 Tian Ruiliang(Shanghai Jianke Technical Assessment of Construction Co.Ltd.,Shanghai 201108,China)
出处 《中国人造板》 2020年第12期26-29,共4页 China Wood-Based Panels
关键词 实木地板 干燥 垫条痕 色差 solid wood flooring drying spacing strips’mark color difference
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部