摘要
以一款市售的40Ah三元离子电池为研究对象,研究其在充放电循环过程一致性的变化、高低温放电性能以及倍率充放电性能。结果表明,随着循环次数的增加,样品的容量一致性变差,低温特性和倍率充电性能变差,而高温放电特性和倍率放电性能基本无衰减。
A 40Ah ternary lithium-ion battery was used as the research object to study its consistency change,high and low temperature discharge performance and rate charge and discharge performance during the charging and discharging cycle.The results show that with the increase of the number of cycles,the consistency of the sample capacity becomes worse,the low temperature characteristic and the rate charge performance become worse,while the high temperature discharge characteristic and the rate discharge performance are basically not attenuated.
作者
龚明光
朱强
范恒斌
Gong Mingguang;Zhu Qiang;Fan Hengbin(不详)
出处
《时代汽车》
2021年第2期121-123,共3页
Auto Time
关键词
锂离子电池
循环
性能
lithium-ion battery
cycle
performance